1. … A Buffer layer is recommended in case of sensitive base material or old unknown layers. OA 67 NiBo can be welded without using protective …
  2. … arc at very low amps. The deposit is free from porosity even on old and or otherwise diluted base material. Preheating is normally done … immediately after welding. … Spheroidal Cast Iron, Diluted Cast Iron, old Cast Iron, Steel to Cast Iron etc.  EN 1561: EN-GJL-100, …
  3. … OA 4370 or OA MnCr is recommended in case of sensible basematerial or old Hardface-layers. … 59-62 HRc hardfacing alloy for cutting edges, …
  4. … A Buffer layer with OA 4370 or OA MnCr is recommended in case of old layers or critical base metals.. … 60-70 HRc Hardfacing wire used …
  5. … resistance. Due to the components Fe, Mn and Sn. this type is the so cold “low fuming bronze”  Flux/Paste: CEWELD Universal-Flux … Brass, …
  6. Brand: Böhler Welding
    CEWELD Product: 347H Tig
    old Thyssen … 235 … Thermanit H-347 …
  7. … Good arc restriking even with cold wire tip, suitable for robot applications. Ideal for use of short …
  8. … of sensitive base material preheating is recommended at 300-400°C. Old Hardfacing layers should be removed, clean or grind properly before …
  9. … in the chemical and petrochemical industry. The low proportion of accompanying elements (Sn, As, Sb, P) in the wire ensures a low Bruscato …
  10. … L-Ag27 is a Very good flowing, low-melting silver hard solder for operating temperatures from -200 °C to Max. 200 °C (without …